Metallurgical Analysis of High Pressure Gas Pipelines Rupture

Authors

  • F. Hasan
  • F. Ahmed

Abstract

On 6 July 2004, two parallel-running gas pipelines (18-inch and 24-inch diameters), in the main transmission network of SNGPL (a gas company in Pakistan) were ruptured. The ruptures occurred in the early hours of the morning about 8 miles downstream of the compressor station AC-4. The ruptures were indicated by the increased gas flow at the outlet of AC-4 [1], first at about 0648 hours and then again about 20 minutes later. The gas escaping from the ruptured lines had caught fire, and the flames had also ‘affected’ a third parallel-running pipeline of 30-inch diameter, lying next to the 24-inch line. The metallurgical examination of the two ruptured lines showed that the 24-inch line was ruptured with the help of an explosive device that had been placed on the underside of the pipe. An examination of the 18-inch line showed that this pipe had failed as a result of the heating of the pipe-wall, presumably, by the flame emanating from the 24-inch line. These two observations clearly suggested that the 24-inch line was the first to rupture (by explosives), and the fire following this rupture had heated the 18-inch pipe to a temperature where its yield strength was unable to support the inside gas pressure. The 20 minutes time interval between the two ruptures was obviously the time taken by the 18-inch pipe to be heated upto the level where it started to yield. The 30-inch line lying next to the 24-inch line was affected to the extent that its coating had been burnt-off over a length of about 40-50 feet. However, the pipe did not exhibit any signs of deshaping or deformation what-so-ever. A replica metallographic examination indicated that the microstructure of the pipe was not measurably affected by the heat. It was thus decided not to replace the ‘affected’ part of the 30-inch pipe, but only to re-coat this affected portion.

References

F. X. R Van Leeuwen; Food and Chemical Toxicology, 38(2000)51-58.

G. Holgate; Environmental and Waste Management, 3(2000)105-112.

G. H. Huang and J. Xia; Journal of Environmental Management, 61(2001)1-23.

Pakistan Millennium Development Goals Report, 2006., Government of Pakistan. Planning Commission., (2006)75. http://www.undp.org.pk/uploaddocuments/mdg2006.zi p. (December 23, 2008)

Global Water Partnership, Draft South Asia - Water Vision 2025, Country Report – Pakistan, (2000).

M. A. Kahlown, M. A. Tahir, H. Rasheed and K. P. Bhatti; Water Quality Status, National Water Quality Monitoring Programme, Fourth Technical Report. Pakistan Council of Research in water Resources, (2006)5.

J. A. Aziz; Eastern Mediterranean Health Journal, 11(2005)1087-1098.

G. Bridges; Asian Water Development Outlook 2007. Country Paper Pakistan, Asian Development Bank,(2007)9. http://www.adb.org/Documents/Books/AWDO/2007/c r08.pdf (December 29, 2008)

Water and Sanitation Program. Managing Karachi's water supply and sanitation services: lessons from a workshop, (2005) 3. http://wwwwds.worldbank.org/external/default/WDSContentServe r/WDSP/IB/2005/11/28/000160016_20051128162902/ Rendered/PDF/344430PK0Karachi0water0supply.pdf

Guidelines for drinking-water quality; 3rd edition, volume 1. World Health Organization (WHO), Geneva, (2004)143-220.

Guidelines for drinking-water quality, 2nd edition, volume 2. World Health Organization (WHO), Geneva, (1996)991.

Standard Methods for the Examination of Water and Wastewater (1998), APHA, AWWA, WEF, Washington D.C.

Downloads

Published

2016-06-22

Issue

Section

Polymer Engineering and Chemical Engineering, Materials Engineering, Physics, Chemistry, Mathematics